Phase diagram of Ti8Co3NiSn4 with Orb v3 conservative inf MPA; e_above_hull: 0.184331 eV/atom; predicted_stable: False
Cell + Ionic relaxation with Orb v3 conservative inf MPA; 0.05 eV/Å threshold; final energy = -109.8613 eV; energy change = -0.9067 eV; symmetry: R-3m → R3m